RFQ Drawing Details That Stop Carbon Fiber Plate Rejects

Sep 28, 2026

Leave a message

RFQ Drawing Details That Stop Carbon Fiber Plate Rejects

Carbon fiber plates machine differently from metal. A drawing that works for aluminium often fails on CFRP. Suppliers need specific notes to protect edges, control tolerances and avoid delamination.

Drawing Items That Prevent Rejects

Drawing Item

Why It Matters for Carbon Fiber Plates

Thickness and tolerance

Controls ply count and layup

Hole diameter and position

Affects drill wander and edge burr

Corner radius

Prevents edge chipping on thin plates

Chamfer or deburr note

Protects exposed plies

Surface finish

Matte or glossy changes machining sequence

Flatness requirement

CFRP moves under clamping force

Minimum RFQ Information

Plate size: length × width × thickness

Material: 3K T300 / T700, epoxy resin

Tolerance: standard ±0.1mm or tighter

Hole map: diameter, position, quantity

Edge treatment: chamfer, deburr, peel ply

Quantity and delivery date

Common Drawing Mistakes

No corner radius on interior cuts

Tight metal tolerances applied to CFRP edges

Missing hole position reference point

Unmarked surface side for matte or glossy

No note on chamfer direction

Supplier Questions Before Production

Which side carries the cosmetic surface?

Are holes through or countersunk?

Is flatness checked before or after cutting?

Are sharp corners acceptable for this application?

FAQ

Q: Do carbon fiber plates need a corner radius?​

A: Yes. Sharp interior corners cause edge chipping. A 0.5mm–1mm radius reduces rejects.

Q: Can suppliers work from a PDF only?​

A: Yes, but DXF or DWG files reduce interpretation errors on hole positions.

Q: What tolerance is realistic on thin plates?​

A: ±0.1mm is standard. ±0.05mm is possible with extra inspection.